| Stainless Steel Balls
BALCO INDUSTRIES
stainless steels offer excellent corrosion resistance in
organic, acid, industrial and marine environments. The
non-magnetic properties combined with exceptionally high
toughness at all temperatures make these steels an
excellent selection for many applications. AISI 302
stainless steel offers superior corrosion resistance due
to the higher nickel and molybdenum content.
|
|
|
--------------------------------------------------------------------------------- |
302
Stainless Steel Balls
Austenitic stainless steels offer excellent corrosion
resistance in organic, acid, industrial and marine
environments. The non-magnetic properties combined with
exceptionally high toughness at all temperatures make
these steels an excellent selection for many applications.
AISI 316 stainless steel offers superior corrosion
resistance due to the higher nickel and molybdenum
content. |
| Material Composition |
|
302
Stainless Steel Balls Material Composition |
| Carbon |
0.15%
max. |
| Manganese |
2.00%
max. |
| Phosphorus |
0.045%
max. |
| Sulfur |
0.030%
max. |
| Silicon |
1.00%
max. |
| Chromium |
17.00
to 19.00% |
| Nickel |
8.00
to 10.00% |
| Nitrogen |
0.10%
max. |
| Copper
(type HQ) |
3.00
to 4.00% |
|
|
| Mechanical Properties |
|
302
Stainless Steel Balls Mechanical Properties |
| Tensile
strength |
100,000
to 180,000 psi |
| Yield
strength |
50,000
to 150,000 psi |
| Elongation
in Two Inches |
55
to 60% |
| Reduction
in Area |
55
to 65% |
| Modulus
of Elasticity |
29,000,000
psi |
| Density |
.286
lbs/cubic inch |
|
|
|
|
|
|
|